I used some West Graphite Powder on my Pygmy bulkhead project. I coated the glass lay-up where it would engage the rubber seals with epoxy/graphite. The result was a fairly hard coating that sanded pretty smooth. Sanding was messy. Wet sanded, it left a trail of blackened water. It was pretty easy to wash up. i am happy with the result: a good seal around the bulkhead flanges. This mixture reminds me of the graphite racing hull paint of the early 70s. One brushed it on the bottom of one's dinghy along with the centerboard and rudder. Then, one could block sand and get a really sweet bottom. Pretty soft, but easy to smooth up. bob phillips SE MI *************************************************************************** PaddleWise Paddling Mailing List - All postings copyright the author and not to be reproduced outside PaddleWise without author's permission Submissions: paddlewise_at_lists.intelenet.net Subscriptions: paddlewise-request_at_lists.intelenet.net Website: http://www.paddlewise.net/ ***************************************************************************Received on Thu Jun 15 2000 - 19:14:49 PDT
This archive was generated by hypermail 2.4.0 : Thu Aug 21 2025 - 16:30:26 PDT