On 21 Dec 2004 at 22:30, Doug Lloyd wrote: > I think the epoxy/glass-tape/gelcoat methodology makes far > more sense. I'd almost agree. If the kayak isn't hull up in the sun a lot, I'd skip the gel coat on the keel. MikeReceived on Wed Dec 22 2004 - 12:19:25 PST