Wes Boyd wrote: > > At 12:25 AM 4/6/00 -0700, Doug Lloyd wrote: > > > > >Back to seams: Then there's the "H" extrusion seam, but let's not go there! > Oh, why not? What don't you like about "H" seams? The way they are done currently, only the inside is taped/glassed, IIRC. The extrusion forms the outside seam. Half the joining strength. Check out what Eddyline does -- not as strong as what Doug is describing. -- Dave Kruger Astoria, OR *************************************************************************** PaddleWise Paddling Mailing List - All postings copyright the author and not to be reproduced outside PaddleWise without author's permission Submissions: paddlewise_at_lists.intelenet.net Subscriptions: paddlewise-request_at_lists.intelenet.net Website: http://www.paddlewise.net/ ***************************************************************************Received on Thu Apr 06 2000 - 07:42:32 PDT