When I owned a plastic yak with that problem, I placed towels over the dimple and poured boiling water on the towels to keep the heat localized. If that doesn't do it, you may need to put pressure on the towels as well. It is possible that the boat was that way from the mold. Then you are SOL. cya *************************************************************************** PaddleWise Paddling Mailing List - Any opinions or suggestions expressed here are solely those of the writer(s). You must assume the entire responsibility for reliance upon them. All postings copyright the author. Submissions: PaddleWise_at_PaddleWise.net Subscriptions: PaddleWise-request_at_PaddleWise.net Website: http://www.paddlewise.net/ ***************************************************************************Received on Thu Apr 26 2001 - 16:40:36 PDT