At 12:50 PM 6/6/2003 -0700, Wayne Smith wrote: > I took Nick Schade's advice, and made something better: I took some West > System epoxy, loaded it up with colloidal silica until it was almost > unworkable, and then added gelcoat pigment and hardener, and made a thick > goo that was just thin enough to flow. I prepped the surface, and painted > it on. 2 seasons, and it barely shows any wear. Wayne, Did you reinforce with any tape? Bill *************************************************************************** PaddleWise Paddling Mailing List - Any opinions or suggestions expressed here are solely those of the writer(s). You must assume the entire responsibility for reliance upon them. All postings copyright the author. Submissions: PaddleWise_at_PaddleWise.net Subscriptions: PaddleWise-request_at_PaddleWise.net Website: http://www.paddlewise.net/ ***************************************************************************Received on Fri Jun 06 2003 - 13:00:23 PDT
This archive was generated by hypermail 2.4.0 : Thu Aug 21 2025 - 16:31:07 PDT